Slurry Settlement

Light curing resin, not used for a long time, color paste is easy to precipitate, will lead to light resin color; If there is a slurry settlement problem, it can be solved by the following methods:

1. Heat the resin in a 60-80℃ oven or other heating container for 30 minutes.

2. After heating for 30 minutes, immediately take out the resin and shake well for about 1 minute.

3. Pour out the resin and observe whether the resin and the original resin are the same color at this time. If the color of the resin is still light, continue to shake it well.