horizontal stripe

Z-axis direction appears in the horizontal pattern.

Machinery: Z-axis line rail or silk lubrication is not enough, stuck and other problems lead to z-axis movement problems, it is recommended to maintain and oil regularly.

Model: The model is placedwithout a drain hole at the bottom. the vacuum pulling is generated during the clamping process, and the clamping force plus vacuum pressure leads to single-layer deformation; the cross-sectional area of the model changes abruptly, such as small area to large area, the clamping force increases and single-layer deformation occurs. Vacuum pulling and abrupt change of cross-sectional area should be avoided as much as possible when placing.

Slicing: the number of support is not enough or too thin, the support is not enough for the model pulling force, the support should be thickened as much as possible, and at the same time, more support should be added to stabilize the model at the cross grain.